PENERAPAN SLAG BAJA SEBAGAI PENGGANTI AGREGAT PADA KARAKTERISTIK SELF COMPACTING CONCRETE

Penulis

  • Adiwijaya Adiwijaya
  • Irka Tangke Datu
  • Khairil Khairil

Abstrak

The aim of this study is to apply steel slag as aggregate on the characteristics of self compacting concrete(SCC). This experimental study was carried out with mixing fresh SCC using iron slag as partial substitution of coarseaggregate and aggregate that were obtained from PT Barawaja in Makassar. Two types of cement binder such as PortlandComposite Cement and Silica Fume are used as binders to produce SCC mixtures. Observation of aggregatecharacteristics and design of SCC concrete mixtures are designed in accordance with SNI 03-2834-1993 and TheEuropean Guidelines for Self-Compacting Concrete. The criteria assessment of SCC concrete were evaluated based onflowability, viscosity and passing ability values of fresh concrete with the testing method Slump flow, V-funnel and Lboxapparatus. Finally, concrete cylinder specimens in dimension of 100 mm in diameter and 200 mm in height werecasted then immersed in water curing. After achievement at 28 days, concrete cylinder specimens were tested incompressive strength according to SNI 1974: 2011. The results concluded that iron slag fulfill the requirements used asraplacement of coarse aggregate and fine aggregate in SCC concrete production with compressive strength of 59.94 MPa.

Diterbitkan

2018-12-30

Terbitan

Bagian

SIPIL & KEAIRAN, TRANSPORTASI, DAN MITIGASI BENCANA